Zirconia-Based Powders Produced by Plasma-Spray Pyrolisys and Properties of Sintered Ceramics

S. N. Kulkov, S. Buyakova, L. A. Gömze

Результат исследований: Материалы для журнала

1 цитирование (Scopus)

Выдержка

It have been studied zirconia-based powders and sintered ceramic. It was shown that in the porous structure of zirconia-based ceramics there is a critical value of porosity the material divides into two sub-systems, being variously deformable under external loading. It have been shown that m-phase in ZrO2 is formed due to increase in the microdistortion level which destabilizes the nanocrystalline t phase. It has been found out the correlation between the sizes of crystallites and porosity, which associated with transition of the isolated porous structure to the continuous one and the porosity of 20%, corresponds to the first percolation threshold.

Язык оригиналаАнглийский
Номер статьи012015
ЖурналJournal of Physics: Conference Series
Том790
Номер выпуска1
DOI
СостояниеОпубликовано - 16 фев 2017
Событие2nd International Conference on Rheology and Modeling of Materials, IC-RMM 2015 - Miskolc-Lillafured, Венгрия
Продолжительность: 5 окт 20159 окт 2015

Отпечаток

zirconium oxides
sprayers
ceramics
porosity
crystallites
thresholds

ASJC Scopus subject areas

  • Physics and Astronomy(all)

Цитировать

Zirconia-Based Powders Produced by Plasma-Spray Pyrolisys and Properties of Sintered Ceramics. / Kulkov, S. N.; Buyakova, S.; Gömze, L. A.

В: Journal of Physics: Conference Series, Том 790, № 1, 012015, 16.02.2017.

Результат исследований: Материалы для журнала

@article{8f8a1d77c2b5403090d7f76805d2461f,
title = "Zirconia-Based Powders Produced by Plasma-Spray Pyrolisys and Properties of Sintered Ceramics",
abstract = "It have been studied zirconia-based powders and sintered ceramic. It was shown that in the porous structure of zirconia-based ceramics there is a critical value of porosity the material divides into two sub-systems, being variously deformable under external loading. It have been shown that m-phase in ZrO2 is formed due to increase in the microdistortion level which destabilizes the nanocrystalline t phase. It has been found out the correlation between the sizes of crystallites and porosity, which associated with transition of the isolated porous structure to the continuous one and the porosity of 20{\%}, corresponds to the first percolation threshold.",
author = "Kulkov, {S. N.} and S. Buyakova and G{\"o}mze, {L. A.}",
year = "2017",
month = "2",
day = "16",
doi = "10.1088/1742-6596/790/1/012015",
language = "English",
volume = "790",
journal = "Journal of Physics: Conference Series",
issn = "1742-6588",
publisher = "IOP Publishing Ltd.",
number = "1",

}

TY - JOUR

T1 - Zirconia-Based Powders Produced by Plasma-Spray Pyrolisys and Properties of Sintered Ceramics

AU - Kulkov, S. N.

AU - Buyakova, S.

AU - Gömze, L. A.

PY - 2017/2/16

Y1 - 2017/2/16

N2 - It have been studied zirconia-based powders and sintered ceramic. It was shown that in the porous structure of zirconia-based ceramics there is a critical value of porosity the material divides into two sub-systems, being variously deformable under external loading. It have been shown that m-phase in ZrO2 is formed due to increase in the microdistortion level which destabilizes the nanocrystalline t phase. It has been found out the correlation between the sizes of crystallites and porosity, which associated with transition of the isolated porous structure to the continuous one and the porosity of 20%, corresponds to the first percolation threshold.

AB - It have been studied zirconia-based powders and sintered ceramic. It was shown that in the porous structure of zirconia-based ceramics there is a critical value of porosity the material divides into two sub-systems, being variously deformable under external loading. It have been shown that m-phase in ZrO2 is formed due to increase in the microdistortion level which destabilizes the nanocrystalline t phase. It has been found out the correlation between the sizes of crystallites and porosity, which associated with transition of the isolated porous structure to the continuous one and the porosity of 20%, corresponds to the first percolation threshold.

UR - http://www.scopus.com/inward/record.url?scp=85016040940&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=85016040940&partnerID=8YFLogxK

U2 - 10.1088/1742-6596/790/1/012015

DO - 10.1088/1742-6596/790/1/012015

M3 - Conference article

AN - SCOPUS:85016040940

VL - 790

JO - Journal of Physics: Conference Series

JF - Journal of Physics: Conference Series

SN - 1742-6588

IS - 1

M1 - 012015

ER -