Hard coatings deposited by physical vapour deposition based on the transition metal nitrides are nowadays widely applied to reduce tool wear. The aim of this paper is to show how microstructural parameters like grain size, stress and chemical and phase composition influence the thermal stability of different hard coatings. This is demonstrated using single-phase coatings like TiN, (Ti, Al, V)N and CrN as well as the dual-phase nanocomposite coatings CrN-Cr2N and TiN-TiB2. It is shown that the resistance against recovery and recrystallization can be improved by introducing a high density of phase boundaries, as is the case for nanocomposite coatings.

Язык оригиналаАнглийский
Страницы (с-по)279-284
Число страниц6
ЖурналUser Modeling and User-Adapted Interaction
Том71
Номер выпуска1-2 SPEC.
DOI
СостояниеОпубликовано - 9 мая 2003

Отпечаток

Hard coatings
Physical vapor deposition
Thermodynamic stability
thermal stability
coatings
Coatings
Nanocomposites
Phase boundaries
nanocomposites
Phase composition
Nitrides
Transition metals
metal nitrides
Wear of materials
Recovery
chemical composition
grain size
transition metals
recovery
vapor deposition

ASJC Scopus subject areas

  • Instrumentation
  • Condensed Matter Physics
  • Surfaces, Coatings and Films

Цитировать

Thermal stability of PVD hard coatings. / Mitterer, C.; Mayrhofer, P. H.; Musil, J.

В: User Modeling and User-Adapted Interaction, Том 71, № 1-2 SPEC., 09.05.2003, стр. 279-284.

Результат исследований: Материалы для журналаСтатья

Mitterer, C. ; Mayrhofer, P. H. ; Musil, J. / Thermal stability of PVD hard coatings. В: User Modeling and User-Adapted Interaction. 2003 ; Том 71, № 1-2 SPEC. стр. 279-284.
@article{d3e2c7b215824dd2b36da382657a8591,
title = "Thermal stability of PVD hard coatings",
abstract = "Hard coatings deposited by physical vapour deposition based on the transition metal nitrides are nowadays widely applied to reduce tool wear. The aim of this paper is to show how microstructural parameters like grain size, stress and chemical and phase composition influence the thermal stability of different hard coatings. This is demonstrated using single-phase coatings like TiN, (Ti, Al, V)N and CrN as well as the dual-phase nanocomposite coatings CrN-Cr2N and TiN-TiB2. It is shown that the resistance against recovery and recrystallization can be improved by introducing a high density of phase boundaries, as is the case for nanocomposite coatings.",
keywords = "Hard coatings, Intrinsic stresses, Microstructure, Recovery, Recrystallization, Thermal stability",
author = "C. Mitterer and Mayrhofer, {P. H.} and J. Musil",
year = "2003",
month = "5",
day = "9",
doi = "10.1016/S0042-207X(02)00751-0",
language = "English",
volume = "71",
pages = "279--284",
journal = "Vacuum",
issn = "0042-207X",
publisher = "Elsevier Limited",
number = "1-2 SPEC.",

}

TY - JOUR

T1 - Thermal stability of PVD hard coatings

AU - Mitterer, C.

AU - Mayrhofer, P. H.

AU - Musil, J.

PY - 2003/5/9

Y1 - 2003/5/9

N2 - Hard coatings deposited by physical vapour deposition based on the transition metal nitrides are nowadays widely applied to reduce tool wear. The aim of this paper is to show how microstructural parameters like grain size, stress and chemical and phase composition influence the thermal stability of different hard coatings. This is demonstrated using single-phase coatings like TiN, (Ti, Al, V)N and CrN as well as the dual-phase nanocomposite coatings CrN-Cr2N and TiN-TiB2. It is shown that the resistance against recovery and recrystallization can be improved by introducing a high density of phase boundaries, as is the case for nanocomposite coatings.

AB - Hard coatings deposited by physical vapour deposition based on the transition metal nitrides are nowadays widely applied to reduce tool wear. The aim of this paper is to show how microstructural parameters like grain size, stress and chemical and phase composition influence the thermal stability of different hard coatings. This is demonstrated using single-phase coatings like TiN, (Ti, Al, V)N and CrN as well as the dual-phase nanocomposite coatings CrN-Cr2N and TiN-TiB2. It is shown that the resistance against recovery and recrystallization can be improved by introducing a high density of phase boundaries, as is the case for nanocomposite coatings.

KW - Hard coatings

KW - Intrinsic stresses

KW - Microstructure

KW - Recovery

KW - Recrystallization

KW - Thermal stability

UR - http://www.scopus.com/inward/record.url?scp=0037427409&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0037427409&partnerID=8YFLogxK

U2 - 10.1016/S0042-207X(02)00751-0

DO - 10.1016/S0042-207X(02)00751-0

M3 - Article

AN - SCOPUS:0037427409

VL - 71

SP - 279

EP - 284

JO - Vacuum

JF - Vacuum

SN - 0042-207X

IS - 1-2 SPEC.

ER -