Peculiarities of modeling of nanoindentation of coating-substrate system

Galina M. Eremina, Alexey Yu Smolin, Sergey G. Psakhie

Результат исследований: Материалы для книги/типы отчетовМатериалы для конференции

1 цитирование (Scopus)

Выдержка

In this paper we discuss some features that are important in modeling nanoindentation of strength coating deposited on metallic substrate. The modeling is performed by movable cellular automaton method, which is a representative of the discrete element methods in computational solid mechanics. Taking into account such factors as capability of the substrate material to harden, friction between the surface and the indenter as well as the presence of an intermediate layer between the coating and the substrate, it is shown that they can deeply affect the mechanical behavior of the system.

Язык оригиналаАнглийский
Название основной публикацииAdvanced Materials with Hierarchical Structure for New Technologies and Reliable Structures
ИздательAmerican Institute of Physics Inc.
Том1683
ISBN (электронное издание)9780735413306
DOI
СостояниеОпубликовано - 27 окт 2015
СобытиеInternational Conference on Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures 2015 - Tomsk, Российская Федерация
Продолжительность: 21 сен 201525 сен 2015

Конференция

КонференцияInternational Conference on Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures 2015
СтранаРоссийская Федерация
ГородTomsk
Период21.9.1525.9.15

Отпечаток

nanoindentation
coating
computational mechanics
solid mechanics
coatings
cellular automata
friction

ASJC Scopus subject areas

  • Physics and Astronomy(all)

Цитировать

Eremina, G. M., Smolin, A. Y., & Psakhie, S. G. (2015). Peculiarities of modeling of nanoindentation of coating-substrate system. В Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures (Том 1683). [020050] American Institute of Physics Inc.. https://doi.org/10.1063/1.4932740

Peculiarities of modeling of nanoindentation of coating-substrate system. / Eremina, Galina M.; Smolin, Alexey Yu; Psakhie, Sergey G.

Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures. Том 1683 American Institute of Physics Inc., 2015. 020050.

Результат исследований: Материалы для книги/типы отчетовМатериалы для конференции

Eremina, GM, Smolin, AY & Psakhie, SG 2015, Peculiarities of modeling of nanoindentation of coating-substrate system. в Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures. том. 1683, 020050, American Institute of Physics Inc., International Conference on Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures 2015, Tomsk, Российская Федерация, 21.9.15. https://doi.org/10.1063/1.4932740
Eremina GM, Smolin AY, Psakhie SG. Peculiarities of modeling of nanoindentation of coating-substrate system. В Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures. Том 1683. American Institute of Physics Inc. 2015. 020050 https://doi.org/10.1063/1.4932740
Eremina, Galina M. ; Smolin, Alexey Yu ; Psakhie, Sergey G. / Peculiarities of modeling of nanoindentation of coating-substrate system. Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures. Том 1683 American Institute of Physics Inc., 2015.
@inproceedings{6b48fe96831240399ffc8b93c1771e8a,
title = "Peculiarities of modeling of nanoindentation of coating-substrate system",
abstract = "In this paper we discuss some features that are important in modeling nanoindentation of strength coating deposited on metallic substrate. The modeling is performed by movable cellular automaton method, which is a representative of the discrete element methods in computational solid mechanics. Taking into account such factors as capability of the substrate material to harden, friction between the surface and the indenter as well as the presence of an intermediate layer between the coating and the substrate, it is shown that they can deeply affect the mechanical behavior of the system.",
author = "Eremina, {Galina M.} and Smolin, {Alexey Yu} and Psakhie, {Sergey G.}",
year = "2015",
month = "10",
day = "27",
doi = "10.1063/1.4932740",
language = "English",
volume = "1683",
booktitle = "Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures",
publisher = "American Institute of Physics Inc.",

}

TY - GEN

T1 - Peculiarities of modeling of nanoindentation of coating-substrate system

AU - Eremina, Galina M.

AU - Smolin, Alexey Yu

AU - Psakhie, Sergey G.

PY - 2015/10/27

Y1 - 2015/10/27

N2 - In this paper we discuss some features that are important in modeling nanoindentation of strength coating deposited on metallic substrate. The modeling is performed by movable cellular automaton method, which is a representative of the discrete element methods in computational solid mechanics. Taking into account such factors as capability of the substrate material to harden, friction between the surface and the indenter as well as the presence of an intermediate layer between the coating and the substrate, it is shown that they can deeply affect the mechanical behavior of the system.

AB - In this paper we discuss some features that are important in modeling nanoindentation of strength coating deposited on metallic substrate. The modeling is performed by movable cellular automaton method, which is a representative of the discrete element methods in computational solid mechanics. Taking into account such factors as capability of the substrate material to harden, friction between the surface and the indenter as well as the presence of an intermediate layer between the coating and the substrate, it is shown that they can deeply affect the mechanical behavior of the system.

UR - http://www.scopus.com/inward/record.url?scp=84984559462&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84984559462&partnerID=8YFLogxK

U2 - 10.1063/1.4932740

DO - 10.1063/1.4932740

M3 - Conference contribution

AN - SCOPUS:84984559462

VL - 1683

BT - Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures

PB - American Institute of Physics Inc.

ER -