Аннотация
It is established that the eliminations of construction sand with the content of SiO<inf>2</inf> about 70 wt.% and particle size less than 60 μm are suitable for the production of a foam-glass–crystal material on the basis of the low-temperature frit, which was synthesized at the temperature of 900°C. The obtained foam-glass–crystal material exceeds foam-glass (by 3.0 times) and clayite (by 1.5 times) by strength and is characterized by the low value of water absorption (0.1%).
Язык оригинала | Английский |
---|---|
Журнал | JOM |
DOI | |
Состояние | Принято/в печати - 6 авг 2015 |
ASJC Scopus subject areas
- Engineering(all)
- Materials Science(all)