Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam

Yu F. Ivanov, K. V. Alsaraeva, E. A. Petrikova, A. D. Teresov, V. E. Gromov, S. V. Konovalov

Результат исследований: Материалы для книги/типы отчетовМатериалы для конференции

4 Цитирования (Scopus)

Выдержка

Irradiation mode has been revealed allowing to increase the silumin fatigue service life in three times, it was established that this fact is caused by the formation of multi-modal, multi-phase, submicro - and nano-structure able to lead to a significant increase in the critical length of crack.

Язык оригиналаАнглийский
Название основной публикацииIOP Conference Series: Materials Science and Engineering
ИздательInstitute of Physics Publishing
Том81
Издание1
DOI
СостояниеОпубликовано - 23 апр 2015
СобытиеInternational Scientific Conference on Radiation-Thermal Effects and Processes in Inorganic Materials, RTEP 2014 - Tomsk, Российская Федерация
Продолжительность: 3 ноя 20148 ноя 2014

Другое

ДругоеInternational Scientific Conference on Radiation-Thermal Effects and Processes in Inorganic Materials, RTEP 2014
СтранаРоссийская Федерация
ГородTomsk
Период3.11.148.11.14

Отпечаток

Fractography
Service life
Electron beams
Irradiation
Fatigue of materials
Cracks

ASJC Scopus subject areas

  • Engineering(all)
  • Materials Science(all)

Цитировать

Ivanov, Y. F., Alsaraeva, K. V., Petrikova, E. A., Teresov, A. D., Gromov, V. E., & Konovalov, S. V. (2015). Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam. В IOP Conference Series: Materials Science and Engineering (1 ред., Том 81). [012011] Institute of Physics Publishing. https://doi.org/10.1088/1757-899X/81/1/012011

Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam. / Ivanov, Yu F.; Alsaraeva, K. V.; Petrikova, E. A.; Teresov, A. D.; Gromov, V. E.; Konovalov, S. V.

IOP Conference Series: Materials Science and Engineering. Том 81 1. ред. Institute of Physics Publishing, 2015. 012011.

Результат исследований: Материалы для книги/типы отчетовМатериалы для конференции

Ivanov, YF, Alsaraeva, KV, Petrikova, EA, Teresov, AD, Gromov, VE & Konovalov, SV 2015, Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam. в IOP Conference Series: Materials Science and Engineering. 1 ред., том. 81, 012011, Institute of Physics Publishing, International Scientific Conference on Radiation-Thermal Effects and Processes in Inorganic Materials, RTEP 2014, Tomsk, Российская Федерация, 3.11.14. https://doi.org/10.1088/1757-899X/81/1/012011
Ivanov YF, Alsaraeva KV, Petrikova EA, Teresov AD, Gromov VE, Konovalov SV. Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam. В IOP Conference Series: Materials Science and Engineering. 1 ред. Том 81. Institute of Physics Publishing. 2015. 012011 https://doi.org/10.1088/1757-899X/81/1/012011
Ivanov, Yu F. ; Alsaraeva, K. V. ; Petrikova, E. A. ; Teresov, A. D. ; Gromov, V. E. ; Konovalov, S. V. / Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam. IOP Conference Series: Materials Science and Engineering. Том 81 1. ред. Institute of Physics Publishing, 2015.
@inproceedings{abfe8382009f437e992a964e2238267c,
title = "Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam",
abstract = "Irradiation mode has been revealed allowing to increase the silumin fatigue service life in three times, it was established that this fact is caused by the formation of multi-modal, multi-phase, submicro - and nano-structure able to lead to a significant increase in the critical length of crack.",
author = "Ivanov, {Yu F.} and Alsaraeva, {K. V.} and Petrikova, {E. A.} and Teresov, {A. D.} and Gromov, {V. E.} and Konovalov, {S. V.}",
year = "2015",
month = "4",
day = "23",
doi = "10.1088/1757-899X/81/1/012011",
language = "English",
volume = "81",
booktitle = "IOP Conference Series: Materials Science and Engineering",
publisher = "Institute of Physics Publishing",
edition = "1",

}

TY - GEN

T1 - Fractography of the fatigue fracture surface of silumin irradiated by high-intensity pulsed electron beam

AU - Ivanov, Yu F.

AU - Alsaraeva, K. V.

AU - Petrikova, E. A.

AU - Teresov, A. D.

AU - Gromov, V. E.

AU - Konovalov, S. V.

PY - 2015/4/23

Y1 - 2015/4/23

N2 - Irradiation mode has been revealed allowing to increase the silumin fatigue service life in three times, it was established that this fact is caused by the formation of multi-modal, multi-phase, submicro - and nano-structure able to lead to a significant increase in the critical length of crack.

AB - Irradiation mode has been revealed allowing to increase the silumin fatigue service life in three times, it was established that this fact is caused by the formation of multi-modal, multi-phase, submicro - and nano-structure able to lead to a significant increase in the critical length of crack.

UR - http://www.scopus.com/inward/record.url?scp=84930451065&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84930451065&partnerID=8YFLogxK

U2 - 10.1088/1757-899X/81/1/012011

DO - 10.1088/1757-899X/81/1/012011

M3 - Conference contribution

AN - SCOPUS:84930451065

VL - 81

BT - IOP Conference Series: Materials Science and Engineering

PB - Institute of Physics Publishing

ER -