Выдержка

The durability of metal-ceramic compositions, including a porcelain fused metal crown, depends on the structure of coverings and pretreatment of the surface of metal. Multicomponent structures are investigated. The influence of separate initial components of a glass bath on masking ability and adhesive strength of glass-ceramic coverings is analyzed.

Язык оригиналаАнглийский
Страницы (с-по)153-159
Число страниц7
ЖурналInorganic Materials: Applied Research
Том2
Номер выпуска2
DOI
СостояниеОпубликовано - апр 2011

Отпечаток

Glass ceramics
Titanium
Metals
Dental Porcelain
Porcelain
Cermets
Chemical analysis
Adhesives
Durability
Glass

ASJC Scopus subject areas

  • Engineering(all)
  • Materials Science(all)

Цитировать

Development of compositions of glass-ceramic coverings for titanium-containing alloys. / Khabas, T. A.; Bol'shanina, T. V.; Kulinich, E. A.; Proskurdin, D. V.

В: Inorganic Materials: Applied Research, Том 2, № 2, 04.2011, стр. 153-159.

Результат исследований: Материалы для журналаСтатья

Khabas, T. A. ; Bol'shanina, T. V. ; Kulinich, E. A. ; Proskurdin, D. V. / Development of compositions of glass-ceramic coverings for titanium-containing alloys. В: Inorganic Materials: Applied Research. 2011 ; Том 2, № 2. стр. 153-159.
@article{f0be62f0d6984ccbb19660588f143ee7,
title = "Development of compositions of glass-ceramic coverings for titanium-containing alloys",
abstract = "The durability of metal-ceramic compositions, including a porcelain fused metal crown, depends on the structure of coverings and pretreatment of the surface of metal. Multicomponent structures are investigated. The influence of separate initial components of a glass bath on masking ability and adhesive strength of glass-ceramic coverings is analyzed.",
keywords = "Adhesive strength, Diopside, Fusible glasses, Hydroxyapatite, Potassium feldspar, Sandblasting, Surface roughness, Wollastonite",
author = "Khabas, {T. A.} and Bol'shanina, {T. V.} and Kulinich, {E. A.} and Proskurdin, {D. V.}",
year = "2011",
month = "4",
doi = "10.1134/S2075113311020122",
language = "English",
volume = "2",
pages = "153--159",
journal = "Inorganic Materials: Applied Research",
issn = "2075-1133",
publisher = "Springer Verlag",
number = "2",

}

TY - JOUR

T1 - Development of compositions of glass-ceramic coverings for titanium-containing alloys

AU - Khabas, T. A.

AU - Bol'shanina, T. V.

AU - Kulinich, E. A.

AU - Proskurdin, D. V.

PY - 2011/4

Y1 - 2011/4

N2 - The durability of metal-ceramic compositions, including a porcelain fused metal crown, depends on the structure of coverings and pretreatment of the surface of metal. Multicomponent structures are investigated. The influence of separate initial components of a glass bath on masking ability and adhesive strength of glass-ceramic coverings is analyzed.

AB - The durability of metal-ceramic compositions, including a porcelain fused metal crown, depends on the structure of coverings and pretreatment of the surface of metal. Multicomponent structures are investigated. The influence of separate initial components of a glass bath on masking ability and adhesive strength of glass-ceramic coverings is analyzed.

KW - Adhesive strength

KW - Diopside

KW - Fusible glasses

KW - Hydroxyapatite

KW - Potassium feldspar

KW - Sandblasting

KW - Surface roughness

KW - Wollastonite

UR - http://www.scopus.com/inward/record.url?scp=80051653862&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=80051653862&partnerID=8YFLogxK

U2 - 10.1134/S2075113311020122

DO - 10.1134/S2075113311020122

M3 - Article

AN - SCOPUS:80051653862

VL - 2

SP - 153

EP - 159

JO - Inorganic Materials: Applied Research

JF - Inorganic Materials: Applied Research

SN - 2075-1133

IS - 2

ER -