In this work, TiSiN coatings were selected to improve the adhesion between dental ceramic and CoCr substrate. The coatings were prepared by the cathodic arc technique in N2 reactive atmosphere, at different bias voltages, and analyzed for elemental composition, surface roughness, wettability and corrosion resistance in Fusayama Meyer artificial saliva. After the coating deposition, low-fusing dental ceramic film was fired on coated alloy, using a dental furnace. The bond strength of these specimens was tested using a 3-point bending test.

Original languageEnglish
Pages (from-to)275-281
Number of pages7
JournalKey Engineering Materials
Volume587
DOIs
Publication statusPublished - 1 Jan 2014
Externally publishedYes
Event25th Symposium and Annual Meeting of the International Society for Ceramics in Medicine, ISCM 2013 - Bucharest, Romania
Duration: 7 Nov 201310 Nov 2013

Fingerprint

Bond strength (materials)
Coatings
Artificial Saliva
Bending tests
Bias voltage
Corrosion resistance
Wetting
Furnaces
Adhesion
Surface roughness
Substrates
Chemical analysis

Keywords

  • Bond strength
  • CoCr
  • Dental materials
  • TiSiN coatings

ASJC Scopus subject areas

  • Materials Science(all)
  • Mechanics of Materials
  • Mechanical Engineering

Cite this

TiSiN coatings for improved bond strength of CoCr alloy to dental ceramic. / Dinu, M.; Braic, V.; Colease, G.; Baciu, F.; Cotrut, C. M.; Braic, M.; Tarcolea, M.; Vitelaru, C.; Vladescu, A.; Vranceanu, D. M.

In: Key Engineering Materials, Vol. 587, 01.01.2014, p. 275-281.

Research output: Contribution to journalConference article

Dinu, M, Braic, V, Colease, G, Baciu, F, Cotrut, CM, Braic, M, Tarcolea, M, Vitelaru, C, Vladescu, A & Vranceanu, DM 2014, 'TiSiN coatings for improved bond strength of CoCr alloy to dental ceramic', Key Engineering Materials, vol. 587, pp. 275-281. https://doi.org/10.4028/www.scientific.net/KEM.587.275
Dinu, M. ; Braic, V. ; Colease, G. ; Baciu, F. ; Cotrut, C. M. ; Braic, M. ; Tarcolea, M. ; Vitelaru, C. ; Vladescu, A. ; Vranceanu, D. M. / TiSiN coatings for improved bond strength of CoCr alloy to dental ceramic. In: Key Engineering Materials. 2014 ; Vol. 587. pp. 275-281.
@article{95150864bda044a8baaef61ec019c570,
title = "TiSiN coatings for improved bond strength of CoCr alloy to dental ceramic",
abstract = "In this work, TiSiN coatings were selected to improve the adhesion between dental ceramic and CoCr substrate. The coatings were prepared by the cathodic arc technique in N2 reactive atmosphere, at different bias voltages, and analyzed for elemental composition, surface roughness, wettability and corrosion resistance in Fusayama Meyer artificial saliva. After the coating deposition, low-fusing dental ceramic film was fired on coated alloy, using a dental furnace. The bond strength of these specimens was tested using a 3-point bending test.",
keywords = "Bond strength, CoCr, Dental materials, TiSiN coatings",
author = "M. Dinu and V. Braic and G. Colease and F. Baciu and Cotrut, {C. M.} and M. Braic and M. Tarcolea and C. Vitelaru and A. Vladescu and Vranceanu, {D. M.}",
year = "2014",
month = "1",
day = "1",
doi = "10.4028/www.scientific.net/KEM.587.275",
language = "English",
volume = "587",
pages = "275--281",
journal = "Key Engineering Materials",
issn = "1013-9826",
publisher = "Trans Tech Publications",

}

TY - JOUR

T1 - TiSiN coatings for improved bond strength of CoCr alloy to dental ceramic

AU - Dinu, M.

AU - Braic, V.

AU - Colease, G.

AU - Baciu, F.

AU - Cotrut, C. M.

AU - Braic, M.

AU - Tarcolea, M.

AU - Vitelaru, C.

AU - Vladescu, A.

AU - Vranceanu, D. M.

PY - 2014/1/1

Y1 - 2014/1/1

N2 - In this work, TiSiN coatings were selected to improve the adhesion between dental ceramic and CoCr substrate. The coatings were prepared by the cathodic arc technique in N2 reactive atmosphere, at different bias voltages, and analyzed for elemental composition, surface roughness, wettability and corrosion resistance in Fusayama Meyer artificial saliva. After the coating deposition, low-fusing dental ceramic film was fired on coated alloy, using a dental furnace. The bond strength of these specimens was tested using a 3-point bending test.

AB - In this work, TiSiN coatings were selected to improve the adhesion between dental ceramic and CoCr substrate. The coatings were prepared by the cathodic arc technique in N2 reactive atmosphere, at different bias voltages, and analyzed for elemental composition, surface roughness, wettability and corrosion resistance in Fusayama Meyer artificial saliva. After the coating deposition, low-fusing dental ceramic film was fired on coated alloy, using a dental furnace. The bond strength of these specimens was tested using a 3-point bending test.

KW - Bond strength

KW - CoCr

KW - Dental materials

KW - TiSiN coatings

UR - http://www.scopus.com/inward/record.url?scp=84900536458&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84900536458&partnerID=8YFLogxK

U2 - 10.4028/www.scientific.net/KEM.587.275

DO - 10.4028/www.scientific.net/KEM.587.275

M3 - Conference article

VL - 587

SP - 275

EP - 281

JO - Key Engineering Materials

JF - Key Engineering Materials

SN - 1013-9826

ER -