Pulsed-arc welding with preheating of electrode extension in the break period

Research output: Contribution to journalArticle

2 Citations (Scopus)

Abstract

A method of pulsed-arc welding with preheating of the electrode in the break between pulses is discussed. The effect of the distance between the contact tips on the melting factor is determined.

Original languageEnglish
Pages (from-to)210-212
Number of pages3
JournalWelding International
Volume29
Issue number3
DOIs
Publication statusPublished - 4 Mar 2015

Fingerprint

Preheating
Electric arc welding
Melting
Electrodes

Keywords

  • device
  • heated
  • pulse-arc welding
  • stick-out

ASJC Scopus subject areas

  • Mechanical Engineering
  • Mechanics of Materials
  • Metals and Alloys

Cite this

Pulsed-arc welding with preheating of electrode extension in the break period. / Krampit, N. Yu; Krampit, Maxim Andreevich.

In: Welding International, Vol. 29, No. 3, 04.03.2015, p. 210-212.

Research output: Contribution to journalArticle

@article{3f25c9ef715946e98cd79cde464351c6,
title = "Pulsed-arc welding with preheating of electrode extension in the break period",
abstract = "A method of pulsed-arc welding with preheating of the electrode in the break between pulses is discussed. The effect of the distance between the contact tips on the melting factor is determined.",
keywords = "device, heated, pulse-arc welding, stick-out",
author = "Krampit, {N. Yu} and Krampit, {Maxim Andreevich}",
year = "2015",
month = "3",
day = "4",
doi = "10.1080/09507116.2014.911408",
language = "English",
volume = "29",
pages = "210--212",
journal = "Welding International",
issn = "0950-7116",
publisher = "Taylor and Francis Ltd.",
number = "3",

}

TY - JOUR

T1 - Pulsed-arc welding with preheating of electrode extension in the break period

AU - Krampit, N. Yu

AU - Krampit, Maxim Andreevich

PY - 2015/3/4

Y1 - 2015/3/4

N2 - A method of pulsed-arc welding with preheating of the electrode in the break between pulses is discussed. The effect of the distance between the contact tips on the melting factor is determined.

AB - A method of pulsed-arc welding with preheating of the electrode in the break between pulses is discussed. The effect of the distance between the contact tips on the melting factor is determined.

KW - device

KW - heated

KW - pulse-arc welding

KW - stick-out

UR - http://www.scopus.com/inward/record.url?scp=84907976603&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84907976603&partnerID=8YFLogxK

U2 - 10.1080/09507116.2014.911408

DO - 10.1080/09507116.2014.911408

M3 - Article

VL - 29

SP - 210

EP - 212

JO - Welding International

JF - Welding International

SN - 0950-7116

IS - 3

ER -