Phase composition of the products of nitriding ferrosilicon with zircon concentrate additives

L. N. Chukhlomina, O. G. Vitushkina, N. N. Golobokov, V. I. Vereshchagin

Research output: Contribution to journalArticle

Abstract

The process of nitride formation during combustion of iron silicon with the addition of zircon concentrate in nitrogen gas is investigated. It is determined that in the presence of zircon (5-70%) ferrosilicon burns in a surface regime, and the products of combustion are multiphase. For the optimal parameters of synthesis (nitrogen pressure 4-7 MPa and sample diameter 35-40 mm) the products of combustion are a composition consisting of a ceramic constituent (Si 3N 4-ZrO 2-Si 2N 2O) and iron (α-Fe). The method of acidic enrichment is used to obtain a composite ceramic powder with iron mass content 0.5%

Original languageEnglish
Pages (from-to)38-40
Number of pages3
JournalGlass and Ceramics (English translation of Steklo i Keramika)
Volume65
Issue number1-2
DOIs
Publication statusPublished - 1 Jan 2008

Fingerprint

Zircon
Nitriding
Phase composition
Nitrogen
Iron
Silicon steel
Nitrides
Powders
Gases
Composite materials
Chemical analysis
zircon
ferrosilicon

ASJC Scopus subject areas

  • Ceramics and Composites
  • Mechanics of Materials
  • Materials Chemistry

Cite this

Phase composition of the products of nitriding ferrosilicon with zircon concentrate additives. / Chukhlomina, L. N.; Vitushkina, O. G.; Golobokov, N. N.; Vereshchagin, V. I.

In: Glass and Ceramics (English translation of Steklo i Keramika), Vol. 65, No. 1-2, 01.01.2008, p. 38-40.

Research output: Contribution to journalArticle

@article{e5dfc39547e34f38847531281b0d6a30,
title = "Phase composition of the products of nitriding ferrosilicon with zircon concentrate additives",
abstract = "The process of nitride formation during combustion of iron silicon with the addition of zircon concentrate in nitrogen gas is investigated. It is determined that in the presence of zircon (5-70{\%}) ferrosilicon burns in a surface regime, and the products of combustion are multiphase. For the optimal parameters of synthesis (nitrogen pressure 4-7 MPa and sample diameter 35-40 mm) the products of combustion are a composition consisting of a ceramic constituent (Si 3N 4-ZrO 2-Si 2N 2O) and iron (α-Fe). The method of acidic enrichment is used to obtain a composite ceramic powder with iron mass content 0.5{\%}",
author = "Chukhlomina, {L. N.} and Vitushkina, {O. G.} and Golobokov, {N. N.} and Vereshchagin, {V. I.}",
year = "2008",
month = "1",
day = "1",
doi = "10.1007/s10717-008-9006-5",
language = "English",
volume = "65",
pages = "38--40",
journal = "Glass and Ceramics (English translation of Steklo i Keramika)",
issn = "0361-7610",
publisher = "Springer New York",
number = "1-2",

}

TY - JOUR

T1 - Phase composition of the products of nitriding ferrosilicon with zircon concentrate additives

AU - Chukhlomina, L. N.

AU - Vitushkina, O. G.

AU - Golobokov, N. N.

AU - Vereshchagin, V. I.

PY - 2008/1/1

Y1 - 2008/1/1

N2 - The process of nitride formation during combustion of iron silicon with the addition of zircon concentrate in nitrogen gas is investigated. It is determined that in the presence of zircon (5-70%) ferrosilicon burns in a surface regime, and the products of combustion are multiphase. For the optimal parameters of synthesis (nitrogen pressure 4-7 MPa and sample diameter 35-40 mm) the products of combustion are a composition consisting of a ceramic constituent (Si 3N 4-ZrO 2-Si 2N 2O) and iron (α-Fe). The method of acidic enrichment is used to obtain a composite ceramic powder with iron mass content 0.5%

AB - The process of nitride formation during combustion of iron silicon with the addition of zircon concentrate in nitrogen gas is investigated. It is determined that in the presence of zircon (5-70%) ferrosilicon burns in a surface regime, and the products of combustion are multiphase. For the optimal parameters of synthesis (nitrogen pressure 4-7 MPa and sample diameter 35-40 mm) the products of combustion are a composition consisting of a ceramic constituent (Si 3N 4-ZrO 2-Si 2N 2O) and iron (α-Fe). The method of acidic enrichment is used to obtain a composite ceramic powder with iron mass content 0.5%

UR - http://www.scopus.com/inward/record.url?scp=49449118818&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=49449118818&partnerID=8YFLogxK

U2 - 10.1007/s10717-008-9006-5

DO - 10.1007/s10717-008-9006-5

M3 - Article

VL - 65

SP - 38

EP - 40

JO - Glass and Ceramics (English translation of Steklo i Keramika)

JF - Glass and Ceramics (English translation of Steklo i Keramika)

SN - 0361-7610

IS - 1-2

ER -