It is established that the eliminations of construction sand with the content of SiO<inf>2</inf> about 70 wt.% and particle size less than 60 μm are suitable for the production of a foam-glass–crystal material on the basis of the low-temperature frit, which was synthesized at the temperature of 900°C. The obtained foam-glass–crystal material exceeds foam-glass (by 3.0 times) and clayite (by 1.5 times) by strength and is characterized by the low value of water absorption (0.1%).

Original languageEnglish
JournalJOM
DOIs
Publication statusAccepted/In press - 6 Aug 2015

Fingerprint

Mortar
Porous materials
Foams
Sand
Water absorption
Temperature
Particle size
Glass

ASJC Scopus subject areas

  • Engineering(all)
  • Materials Science(all)

Cite this

Low-Temperature Synthesis of Porous Materials from Mortar Sands. / Kazmina, O. V.; Volland, S. N.; Dushkina, M. A.

In: JOM, 06.08.2015.

Research output: Contribution to journalArticle

@article{154be52ff9eb4c2a87a263b956d37ca0,
title = "Low-Temperature Synthesis of Porous Materials from Mortar Sands",
abstract = "It is established that the eliminations of construction sand with the content of SiO2 about 70 wt.{\%} and particle size less than 60 μm are suitable for the production of a foam-glass–crystal material on the basis of the low-temperature frit, which was synthesized at the temperature of 900°C. The obtained foam-glass–crystal material exceeds foam-glass (by 3.0 times) and clayite (by 1.5 times) by strength and is characterized by the low value of water absorption (0.1{\%}).",
author = "Kazmina, {O. V.} and Volland, {S. N.} and Dushkina, {M. A.}",
year = "2015",
month = "8",
day = "6",
doi = "10.1007/s11837-015-1554-x",
language = "English",
journal = "JOM",
issn = "1047-4838",
publisher = "Minerals, Metals and Materials Society",

}

TY - JOUR

T1 - Low-Temperature Synthesis of Porous Materials from Mortar Sands

AU - Kazmina, O. V.

AU - Volland, S. N.

AU - Dushkina, M. A.

PY - 2015/8/6

Y1 - 2015/8/6

N2 - It is established that the eliminations of construction sand with the content of SiO2 about 70 wt.% and particle size less than 60 μm are suitable for the production of a foam-glass–crystal material on the basis of the low-temperature frit, which was synthesized at the temperature of 900°C. The obtained foam-glass–crystal material exceeds foam-glass (by 3.0 times) and clayite (by 1.5 times) by strength and is characterized by the low value of water absorption (0.1%).

AB - It is established that the eliminations of construction sand with the content of SiO2 about 70 wt.% and particle size less than 60 μm are suitable for the production of a foam-glass–crystal material on the basis of the low-temperature frit, which was synthesized at the temperature of 900°C. The obtained foam-glass–crystal material exceeds foam-glass (by 3.0 times) and clayite (by 1.5 times) by strength and is characterized by the low value of water absorption (0.1%).

UR - http://www.scopus.com/inward/record.url?scp=84938702277&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84938702277&partnerID=8YFLogxK

U2 - 10.1007/s11837-015-1554-x

DO - 10.1007/s11837-015-1554-x

M3 - Article

JO - JOM

JF - JOM

SN - 1047-4838

ER -