Leaded-tin bronze destruction mechanism

Research output: Chapter in Book/Report/Conference proceedingConference contribution

11 Citations (Scopus)

Abstract

The paper is devoted to comparative analysis of the structure and mechanical properties of leaded-tin bronze with lead inclusions of various morphologies. In order to obtain lead inclusions of certain morphology, casts are cooled at certain velocities. Low cooling velocities cause spheroidizing of lead inclusions, whereas high ones give prolate inclusions with torn uneven surface.

Original languageEnglish
Title of host publicationProceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012
DOIs
Publication statusPublished - 2012
Event2012 7th International Forum on Strategic Technology, IFOST 2012 - Tomsk, Russian Federation
Duration: 18 Sep 201221 Sep 2012

Other

Other2012 7th International Forum on Strategic Technology, IFOST 2012
CountryRussian Federation
CityTomsk
Period18.9.1221.9.12

Fingerprint

Bronze
Tin
Lead
Cooling
Mechanical properties
Inclusion

Keywords

  • bronze
  • destruction
  • destruction mechanism
  • fusible phase
  • lead inclusions
  • leaded-tin bronze

ASJC Scopus subject areas

  • Management of Technology and Innovation

Cite this

Martyushev, N. V. (2012). Leaded-tin bronze destruction mechanism. In Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012 [6357597] https://doi.org/10.1109/IFOST.2012.6357597

Leaded-tin bronze destruction mechanism. / Martyushev, N. V.

Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012. 2012. 6357597.

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Martyushev, NV 2012, Leaded-tin bronze destruction mechanism. in Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012., 6357597, 2012 7th International Forum on Strategic Technology, IFOST 2012, Tomsk, Russian Federation, 18.9.12. https://doi.org/10.1109/IFOST.2012.6357597
Martyushev NV. Leaded-tin bronze destruction mechanism. In Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012. 2012. 6357597 https://doi.org/10.1109/IFOST.2012.6357597
Martyushev, N. V. / Leaded-tin bronze destruction mechanism. Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012. 2012.
@inproceedings{0fef66fc3a824916811a242257ca4eb1,
title = "Leaded-tin bronze destruction mechanism",
abstract = "The paper is devoted to comparative analysis of the structure and mechanical properties of leaded-tin bronze with lead inclusions of various morphologies. In order to obtain lead inclusions of certain morphology, casts are cooled at certain velocities. Low cooling velocities cause spheroidizing of lead inclusions, whereas high ones give prolate inclusions with torn uneven surface.",
keywords = "bronze, destruction, destruction mechanism, fusible phase, lead inclusions, leaded-tin bronze",
author = "Martyushev, {N. V.}",
year = "2012",
doi = "10.1109/IFOST.2012.6357597",
language = "English",
isbn = "9781467317702",
booktitle = "Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012",

}

TY - GEN

T1 - Leaded-tin bronze destruction mechanism

AU - Martyushev, N. V.

PY - 2012

Y1 - 2012

N2 - The paper is devoted to comparative analysis of the structure and mechanical properties of leaded-tin bronze with lead inclusions of various morphologies. In order to obtain lead inclusions of certain morphology, casts are cooled at certain velocities. Low cooling velocities cause spheroidizing of lead inclusions, whereas high ones give prolate inclusions with torn uneven surface.

AB - The paper is devoted to comparative analysis of the structure and mechanical properties of leaded-tin bronze with lead inclusions of various morphologies. In order to obtain lead inclusions of certain morphology, casts are cooled at certain velocities. Low cooling velocities cause spheroidizing of lead inclusions, whereas high ones give prolate inclusions with torn uneven surface.

KW - bronze

KW - destruction

KW - destruction mechanism

KW - fusible phase

KW - lead inclusions

KW - leaded-tin bronze

UR - http://www.scopus.com/inward/record.url?scp=84871823718&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84871823718&partnerID=8YFLogxK

U2 - 10.1109/IFOST.2012.6357597

DO - 10.1109/IFOST.2012.6357597

M3 - Conference contribution

SN - 9781467317702

BT - Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012

ER -