Electrical properties of lithium ferrite with addition of ZrO2

Research output: Contribution to journalConference article

2 Citations (Scopus)

Abstract

The study of electrical properties of composite ceramics based on lithium ferrite LiFe5O8 with the addition of ZrO2 (1 and 2 wt%) was carried out. The samples were prepared by standard ceramic technology. Synthesis of lithium ferrite was conducted at 800°C for 120 minutes. The zirconium dioxide was added to synthesized powder by mixing in planetary ball mill, and then the composite powders were sintered at temperatures of 1100°C and 1050°C. The electrical conductivity of the samples was studied using two-probe spreading resistance method. It was found that addition of ZrO2 and an increase of its up to 2 wt% leads to increase in the activation energy and electrical resistivity.

Original languageEnglish
Article number012091
JournalIOP Conference Series: Materials Science and Engineering
Volume110
Issue number1
DOIs
Publication statusPublished - 23 Feb 2016
Event11th International Scientific Conference on Radiation-Thermal Effects and Processes in Inorganic Materials 2015, RTEP 2015 - Tomsk, Russian Federation
Duration: 31 Aug 201510 Sep 2015

Fingerprint

Lithium
Powders
Ferrite
Electric properties
Ball mills
Composite materials
Zirconium
Activation energy
Temperature
zirconium oxide
Electric Conductivity

ASJC Scopus subject areas

  • Materials Science(all)
  • Engineering(all)

Cite this

Electrical properties of lithium ferrite with addition of ZrO2. / Lamonova, S. A.; Surzhikov, Anatoly Petrovich; Lysenko, E. N.

In: IOP Conference Series: Materials Science and Engineering, Vol. 110, No. 1, 012091, 23.02.2016.

Research output: Contribution to journalConference article

@article{39347b70c8fc4a61b87ae0e5a48c33b8,
title = "Electrical properties of lithium ferrite with addition of ZrO2",
abstract = "The study of electrical properties of composite ceramics based on lithium ferrite LiFe5O8 with the addition of ZrO2 (1 and 2 wt{\%}) was carried out. The samples were prepared by standard ceramic technology. Synthesis of lithium ferrite was conducted at 800°C for 120 minutes. The zirconium dioxide was added to synthesized powder by mixing in planetary ball mill, and then the composite powders were sintered at temperatures of 1100°C and 1050°C. The electrical conductivity of the samples was studied using two-probe spreading resistance method. It was found that addition of ZrO2 and an increase of its up to 2 wt{\%} leads to increase in the activation energy and electrical resistivity.",
author = "Lamonova, {S. A.} and Surzhikov, {Anatoly Petrovich} and Lysenko, {E. N.}",
year = "2016",
month = "2",
day = "23",
doi = "10.1088/1757-899X/110/1/012091",
language = "English",
volume = "110",
journal = "IOP Conference Series: Materials Science and Engineering",
issn = "1757-8981",
publisher = "IOP Publishing Ltd.",
number = "1",

}

TY - JOUR

T1 - Electrical properties of lithium ferrite with addition of ZrO2

AU - Lamonova, S. A.

AU - Surzhikov, Anatoly Petrovich

AU - Lysenko, E. N.

PY - 2016/2/23

Y1 - 2016/2/23

N2 - The study of electrical properties of composite ceramics based on lithium ferrite LiFe5O8 with the addition of ZrO2 (1 and 2 wt%) was carried out. The samples were prepared by standard ceramic technology. Synthesis of lithium ferrite was conducted at 800°C for 120 minutes. The zirconium dioxide was added to synthesized powder by mixing in planetary ball mill, and then the composite powders were sintered at temperatures of 1100°C and 1050°C. The electrical conductivity of the samples was studied using two-probe spreading resistance method. It was found that addition of ZrO2 and an increase of its up to 2 wt% leads to increase in the activation energy and electrical resistivity.

AB - The study of electrical properties of composite ceramics based on lithium ferrite LiFe5O8 with the addition of ZrO2 (1 and 2 wt%) was carried out. The samples were prepared by standard ceramic technology. Synthesis of lithium ferrite was conducted at 800°C for 120 minutes. The zirconium dioxide was added to synthesized powder by mixing in planetary ball mill, and then the composite powders were sintered at temperatures of 1100°C and 1050°C. The electrical conductivity of the samples was studied using two-probe spreading resistance method. It was found that addition of ZrO2 and an increase of its up to 2 wt% leads to increase in the activation energy and electrical resistivity.

UR - http://www.scopus.com/inward/record.url?scp=84971596866&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84971596866&partnerID=8YFLogxK

U2 - 10.1088/1757-899X/110/1/012091

DO - 10.1088/1757-899X/110/1/012091

M3 - Conference article

VL - 110

JO - IOP Conference Series: Materials Science and Engineering

JF - IOP Conference Series: Materials Science and Engineering

SN - 1757-8981

IS - 1

M1 - 012091

ER -